Features | Benefits and Applications |
---|---|
|
|
|
|
Characteristics |
Conditions |
Specified values |
Units |
---|---|---|---|
Geometry Characteristics |
|||
Core Diameter |
-- |
62.5±2.5 |
[μm] |
Core Non-Circularity |
-- |
≤5.0 |
[%] |
Cladding Diameter |
-- |
125.0±1.0 |
[μm] |
Cladding Non-Circularity |
-- |
≤1.0 |
[%] |
Coating Diameter |
-- |
245±7 |
[μm] |
Coating/Cladding Concentricity Error |
-- |
≤10.0 |
[μm] |
Coating Non-Circularity |
-- |
≤6.0 |
[%] |
Core/Cladding Concentricity Error |
-- |
≤1.5 |
[μm] |
Delivery Length |
-- |
up to 17.6 |
[km/reel] |
Optical Characteristics |
|||
Attenuation |
850nm |
≤2.7 |
[dB/km] |
1300nm |
≤0.6 |
[dB/km] |
|
Overfilled Modal Bandwidth |
850nm |
≥200 |
[MHz·km] |
1300nm |
≥500 |
[MHz·km] |
|
Numerical Aperture |
-- |
0.275±0.015 |
-- |
Group Refractive Index |
850nm |
1.496 |
-- |
1300nm |
1.491 |
-- |
|
Zero Dispersion Wavelength,λ0 |
-- |
1320~1365 |
[nm] |
Zero Dispersion Slope,S0 |
1320nm≤ λ0 ≤1348nm |
≤0.11 |
[ps/(nm2·km)] |
1348nm≤ λ0 ≤1365nm |
≤0.001(1458-λ0 ) |
[ps/(nm2·km)] |
|
Macrobending Loss |
-- |
-- |
-- |
100 Turns @ 37.5 mm Radius |
850nm |
≤0.50 |
[dB] |
1300nm |
≤0.50 |
[dB] |
|
Backscatter Characteristics |
1300nm | ||
Step(Mean of Bidirectional Measurement) |
-- |
≤0.10 |
[dB] |
Irregularities Over Fibre Length and Point Discontinuity |
-- |
≤0.10 |
[dB] |
Attenuation Uniformity |
-- |
≤0.10 |
[dB/km] |
Environmental Characteristics |
850nm & 1300nm | ||
Temperature Cycling |
-60℃ to 85℃ |
≤0.10 |
[dB/km] |
Temperature-Humidity Cycling |
-10℃ to 85℃,4% to 98% RH |
≤0.10 |
[dB/km] |
Water Immersion |
23℃, 30 days |
≤0.10 |
[dB/km] |
Dry Heat |
85℃,30 days |
≤0.10 |
[dB/km] |
Damp Heat |
85℃, 85% RH,30 days |
≤0.10 |
[dB/km] |
Mechanical Specification |
|||
Proof Test |
-- |
≥9.0 |
[N] |
-- |
≥1.0 |
[%] |
|
-- |
≥100 |
[kpsi] |
|
Coating Strip Force |
typical average force |
1.5 |
[N] |
peak force |
≥1.3,≤8.9 |
[N] |
|
Dynamic Stress Corrosion Susceptibility Parameter(nd, typical) | -- |
20 |
-- |