• YOFC radiation resistant fibre complies with orexceeds ITU-T.G651 & IEC 60793-2-10 A1a fibre specification.
• The fibre is produced by plasma activated chemical vapor deposition (PCVD) process. the radiation resistant multi mode fibre fabricated by PCVD process has excellent radiation resistant properties at 850nm& 1300nm based on its special glass components and manufacturing proces
• Due to the accurate control of deposition of PCVD process, YOFC radiation resistant multi-mode fibre has perfect waveguide refractive index profile, which guarantees the excellent geometrical, attenuation and bandwidth characteristics
• Stable transmission property under radiation environment
• High bandwidth and low attenuation @ 850nm & 1300nm
• Good stripping and welding Properties
• Suitable for various cable structures and favorable for tight/loose tubes
Fibre Type |
RDG 50/125 |
|
---|---|---|
Part No. |
RD2011-A |
|
Optical Properties |
||
Attenuation@850/1300nm(dB/km) |
2.5/1.0 |
|
Bandwidth@850/1300nm(MHz·km) |
300/300 |
|
Numerical Aperture |
0.2± 0.015 |
|
Geometrical Properties |
||
Core Diameter(μm) |
50 ±2.5 |
|
Cladding Diameter(μm) |
125 ±1 |
|
Coating Diameter(μm) |
245 ±10 |
|
Core/Cladding Concentricity(μm) |
≤1 |
|
Core Non-circularity(%) |
≤3 |
|
Coating/Clad Concentricity(μm) |
≤10 |
|
Cladding Non-Circularity(%) |
≤0.7 |
|
Spool Length(km) |
1.1~8.8 |
|
Material Composition |
||
Core Material |
F Doped Silica Glass |
|
Cladding Material |
Pure Silica Glass |
|
Coating Material |
Dual-layer UV-Acrylate |
|
Environmental Properties |
||
Temperature Induced Loss(dB/km) |
≤0.2 |
|
Temperature-humidity Cycling Induced Attenuation(dB/km) |
≤0.2 |
|
Watersoak Dependence Induced Attenuation (dB/km) |
≤0.2 |
|
Damp Heat Dependence Induced Attenuation(dB/km) |
≤0.2 |
|
Dry Heat Aging (dB/km) |
≤0.2 |
|
Mechanical Properties |
||
Proof Test Level(kpsi) |
≥75 |
|
Strip Force(N) |
1.2 |
|
≥1.2 ≤8.9 |
||
Dynamic Stress Corrosion Susceptibility Parameter nd |
≥24 |
|
Radiation-resistance Characteristcics |
||
According to TIA/EIA 455-64(dB/km) |
Total dose :250kGy,dose rate: 1Gy/s(25°C), induced attenuation@1310nm |
≤15 |